Design guide for overmolding
What you need to know to design a part for overmolding, explained simply, each with a diagram. No molding knowledge needed.
The shape of the overmold
The notions that come up in the analysis of your part.
-
The parting line: where the mold opens An overmolding mold is made of two halves. Knowing where they meet helps you read almost every other point of the analysis. Read
-
Shapes that trap the part (undercuts) A part must be able to come straight out of the mold. An undercut is a shape that prevents it. Read
-
Wall slope (draft angle) A slightly tilted wall releases from the mold without rubbing. Read
-
Resin thickness over your components The resin protects your components only where it is thick enough. Read
-
Even resin thickness Neither too thick nor too thin: resin of even thickness gives the best-looking part. Read
-
Cable exits A cable holds and stays sealed if it is held far enough into the resin and exits at the right place. Read
-
Holding the components in the mold During injection, the resin pushes on your components: they must be held in place. Read
Wiring and the board
For a custom connector, splitter or harness: what is decided when drawing the board and choosing the cable, even before the shape of the overmold.
-
Solder pads in line with the cable A wire soldered in line with the cable puts no strain on its solder joint. Read
-
Connecting the shields A shield is a bare conductor: it needs its own pad, at the edge of the board. Read
-
Branching without a board (splices) When a conductor splits in two without a board, the joint sits inside the overmold: staggered, sleeved, away from where the cable bends. Read
-
The path of the wires to the connector Between the end of the jacket and the connector, nothing holds the wires: the shorter and straighter this path, the better they stay in the heart of the resin. Read
-
Choosing a cable that overmolds well The resin comes in hot and has to bond to the cable: the material of its jacket and of its insulation decides both. Read
-
An assembly that can be checked at every step A fault found before injection can be fixed; afterward, it is sealed in the resin. Read
-
What your drawings should specify What a drawing does not say, the shop has to assume: better to write it down. Read
Designing an overmoldable part
The values to aim for, file preparation and the steps, on a single page.